I finally stopped normalizing my coal fire before hammering, and my welds stopped cracking
Last month I was forging a set of tongs out of 3/8 inch square stock and kept getting cracks along the reins, so I asked an old timer at the Guild meetup in Asheville what I was missing. He pointed out that most beginners, me included, pull the steel out of the fire when it looks orange but the core is still cold, and normalizing at that point just sets up stress fractures later. I started soaking the stock an extra 45 seconds past the orange glow, and the last 6 tongs came out clean with zero cracks. Curious if anyone else here judges heat by color alone or if you go by feel and sound of the hammer.